Manufacturer, trader & exporter · Girgaon, Mumbai · ISO 9001:2015 certifiedEN ES PT العربية · +91 99207 55510 · WhatsApp · sales@kanaksteeleng.com
MS / CS & Alloy Steel · P22

ASTM A335 P22 — Pipe & Tube, Fittings & Flanges

Also sold as SA-335 P22 · 2¼Cr-1Mo alloy pipe · UNS K21590

ASTM A335 P22 is a chrome-moly alloy steel pipe for high-temperature, high-pressure service, chosen for high-pressure steam and hydrogen service up to about 580 °C. We manufacture, trade and export it as pipe & tube, fittings, flanges; EN 10204 3.1 or 3.2 certificates are available on request / as specified in the PO. Markets we have supplied to include Oman, UAE, Saudi Arabia, Brazil, Argentina, Spain and Chile (India is the home market).

  • P22
  • ρ 7.85 g/cm³

Reviewed by the Kanak Steel & Engineering Co. technical team · Updated November 2026

Price & availability

Chat on WhatsApp

Quotations within one working day, in INR or USD.

ASTM A335 P22 Specifications by Product — Which Standard Applies?

The material standard changes with the product form. This is the table buyers ask for most.

ProductMaterial standardDimensions
ASTM A335 P22 pipe & tubeASTM A335 P22ASME B36.19 / B36.10
ASTM A335 P22 fittingsASTM A234 WP22 · ASTM A182 F22ASME B16.9 · B16.11
ASTM A335 P22 flangesASTM A182 F22ASME B16.5 · B16.47

ASTM A335 P22 Chemical Composition

Under technical review for TDS.

ElementCurrent requirement
Chromium1.90 – 2.60
Molybdenum0.87 – 1.13
Carbon0.05 – 0.15
Manganese0.30 – 0.60
Silicon0.50 max
Phosphorus0.025 max
Sulphur0.025 max

Numerical specification requirements are published only after the applicable current standard edition has been verified. Governing specification to be verified: ASTM A335 Grade P22.

ASTM A335 P22 Mechanical Properties

Under technical review for TDS.

PropertyCurrent requirement
Tensile strength415 MPa (60 ksi) min
Yield strength 0.2%205 MPa (30 ksi) min
Elongation30 % longitudinal / 20 % transverse (basic minimum, in 50 mm)

Numerical specification requirements are published only after the applicable current standard edition has been verified. Governing specification and condition to be verified: ASTM A335 Grade P22 — condition per order.

Density & Physical Properties

PropertyValue
Density7.85 g/cm³
Melting range1420 – 1530 °C
MagneticMagnetic

ASTM A335 P22 Equivalent Grades

DesignationASTM A335 P22
Also calledSA-335 P22 · 2¼Cr-1Mo alloy pipe · UNS K21590
StandardASTM A335 Grade P22

Welding ASTM A335 P22

Matching fillerER90S-B3 / E9018-B3
Also usedPreheat and PWHT per ASME B31.1 / B31.3

ASTM A335 P22 for export

FOB / CIF · Nhava Sheva (JNPT), Mumbai · markets supplied to
Confirmed export markets

India is the home market. No overseas offices or warehouses are claimed.

ASTM A335 P22 — questions buyers ask

What is ASTM A335 P22?

ASTM A335 P22 is a chrome-moly alloy steel pipe for high-temperature, high-pressure service. It is chosen for high-pressure steam and hydrogen service up to about 580 °C.

Which standards cover ASTM A335 P22 products?

Pipe & Tube: ASTM A335 P22; Fittings: ASTM A234 WP22 · ASTM A182 F22; Flanges: ASTM A182 F22. Always name the standard and edition on your order.

What is the density of ASTM A335 P22?

7.85 g/cm³ — use it to calculate weights: plate kg = L(m) × W(m) × t(mm) × 7.85.

Reviewed by the technical team, Kanak Steel & Engineering Co.
Sources: the ASTM / ASME specifications named on this page and producer datasheets · Last updated November 2026